Republication

No entries were found.
Republication Author Republication date Publisher
燃煤机组烟气深度冷却增效减排技术 赵钦新 严俊杰 王云刚 姜衍更 刘明 梁志远 2018-04-01 中国电力出版社
余热锅炉研究与设计 赵钦新 周屈兰 谭厚章 惠世恩 2010-09-22 中国标准出版社
超临界锅炉耐热钢研究 赵钦新 朱丽慧 2010-01-04 机械工业出版社
工业锅炉安全经济运行 赵钦新 2003-02-27 北京:中国标准出版社
燃油燃气锅炉结构设计及图册 赵钦新 李卫东 惠世恩 2002-08-06 西安交通大学出版社
.燃油燃气锅炉 赵钦新 惠世恩 2000-06-07 西安交通大学出版社

Blank2

2018

  1. Shao H, Zhao Q, Liang Z, et al. Numerical investigation on a separated structure shell-and-tube waste heat boiler based on experiment[J]. International Journal of Heat and Mass Transfer, 2018, 117: 1006-1018.
  2.  Liang Z, Yu M, Xu Z, et al. Influence of Low-Temperature Pre-oxidation by Ozone on Corrosion Resistance of T91 Steel in Steam at 600° C[J]. Oxidation of Metals, 1-10.
  3.  Pan P, Chen H, Liang Z, et al. Deposition and corrosion characteristics of liquid-solid droplets on tubular corrosion probes in desulfurized flue gas[J]. Engineering Failure Analysis, 2018, 90: 129-140.
  4.  Liang Z, Zhao Q, Deng J, et al. Influence of Aging treatment on the microstructure and mechanical properties of T92/Super 304H dissimilar metal welds[J]. Materials at High Temperatures, 2018, 35 (4): 327-334.
  5.  于淼,梁志远,桂雍等. 4种先进超超临界电站锅炉用高温合金高温腐蚀性能实验研究[J].表面技术,2018476):8-16.
  6.  Liang Z, Wang Y, Zhao Q. Steam oxidation behavior of alloy 617 at 900°C to 1100°C[J]. Metallurgical and Materials Transactions A, 2018, 49(7): 3133–3144.
  7.  Liang Z, Yu M, Gui Y, et al. Corrosion behavior of heat-resistant materials in the high-temperature carbon dioxide environment[J]. JOM, 2018.
  8.  梁志远,于淼,桂雍,赵钦新. 高温二氧化碳环境下耐热合金腐蚀行为研究[J]. 腐蚀科学与防护技术,2018303),237-243.

 2017

  1. Pan P Y, Chen H, Liang Z Y, et al. Experimental study on corrosion of steels for flue gas reheaters in a coal-fired power plant[J]. Applied Thermal Engineering, 2017, 115: 267-279.
  2.  Liang Z, Sha W, Zhao Q, et al. The Effect of Aging Heat Treatment on the Microstructure and Mechanical Properties of 10Cr20Ni25Mo1. 5NbN Austenitic Steel[J]. High Temperature Materials and Processes, 2016, 35(1): 1-7.
  3.  Hong X, Zhiyuan L, Jianliang D, et al. Effect of Pre-Oxidation on the Steam Oxidation of Heat-Resistant Steel T92[J]. High Temperature Materials and Processes.
  4.  Chen X, Zhao Q, Liang Z. Investigations on the Ash Deposit Formation of Tubular Air Preheater in a Coal-Fired Traveling Grate Boiler[J]. Energy & Fuels, 2017, 31(12): 13215-13220.
  5.  Chen L, Li Y, Zhao Q, et al. Removal of NOX Using Hydrogen Peroxide Vapor over Fe/TiO2 Catalysts and an Absorption Technique[J]. Catalysts, 2017, 7(12): 38

 2016

  1. Liang Zhiyuan, Singh P M, Zhao Q, et al. High Temperature Oxidation of Newly Developed Alloy 282 in the Flowing-Air and Steam Condition at 900–1100° C[J]. Oxidation of Metals, 2015, 84(3-4): 291-305. (SCI: CQ8VG)
  2.  Liang Zhiyuan, Zhao Q, Singh P M, et al. Field studies of steam oxidation behavior of austenitic heat-resistant steel 10Cr18Ni9Cu3NbN[J]. Egineering Failure Analysis, 2015, 53: 132-137. (SCI: CG5UI)
  3.  Liang Zhiyuan, Zhao Qinxin,Wang Yungang, et al. Coupling mechanism of dew point corrosion and viscous ash deposits. Materials and Corrosion-werkstoffe Und Korrosion, 2014, 65(8):797-802.  (SCI: AN3ZA)
  4.  Liang Zhiyuan, Jin X, Zhao Q. Investigation of overheating of the final super-heater in a 660MW power plant[J]. Engineering Failure Analysis, 2014, 45: 59-64. (SCI: AO5AY)
  5.  Liang Zhiyuan, Sha W, Zhao Q, et al. The Effect of Aging Heat Treatment on the Microstructure and Mechanical Properties of 10Cr20Ni25Mo1. 5NbN Austenitic Steel[J]. High Temperature Materials and Processes, 2016, 35(1): 1-7. (SCI: DA6UN)
  6.  Liang Zhiyuan, Zhao Qinxin. Failure analysis of spiral finned tube on the economizer. Engineering Failure Analysis, 2013, 28:208-214.  (SCI: 107RY)
  7.  Sha W, Liang Zhiyuan, Zhao Q, et al. High temperature corrosion of typical positions in SUS 30432 tubing bend tested in simulated environment[J]. Materials at High Temperatures, 2015, 32(4): 419-425. (SCI: CH4VD)
  8.  Deng J, Liang Zhiyuan, Hui S, et al. Aging Treatment on the Microstructures and Mechanical Properties of New Groove T92/Super 304H Dissimilar Steel Joints[J]. High Temperature Materials and Processes, 2015, 34(5): 425-433. (SCI: CN3LK)
  9.  Wang Y G, Zhao Q X, Liang Zhiyuan, et al. Analysis on high-temperature corrosion characteristic of 10Cr18Ni9NbCu3BN steel[J]. Materials Research Innovations, 2015, 19: 104-108. (SCI: CI7QA)
  10.  Wang Y, Ma H, Liang Zhiyuan, et al. Experimental study on dew point corrosion characteristics of the heating surface in a 65 t/h biomass-fired circulating fluidized bed boiler[J]. Applied Thermal Engineering, 2016, 96: 76-82.  (SCI: DJ0AI)
  11.  Zhao Q, Liang Zhiyuan, Jiang W. Studies on High Temperature Corrosion of Austenitic HeatResistant Steels Super 304H/10Cr18Ni9Cu3NbN in Simulated and Real Combustion Gas Atmospheres[J]. Energy Materials 2014, 243-250. (EI: 2700998988)
  12.  Liang Zhiyuan, Zhao Q X. Research on Dew Point Corrosion of Materials[J]. Applied Mechanics and Materials. 2013, 281: 441-447.(EI:0515979800)
  13.  Liang Zhiyuan, Singh PM, Zhao Qinxin, Effect of pre-oxdiation on the steam oxidation of T92 steel at 650[C], NACE 2015, 2015, Dallas.
  14.  Liang Zhiyuan, Zhao Qinxin, Singh PM, Oxidation of Fe-Ni-base alloy HR120 and Ni-base alloy 282 in Steam Environment at 800 to 1000[C], NACE 2016, 2016, Vancouver.
  15.  Liang Zhiyuan, Zhao Qinxin, Singh PMHigh temperature oxidation of several austenitic steels and nickel-based super-alloys in steam environment [C]. 8th International Conference on Advances in Materials Technology for Fossil Power Plants, 2016, Portugal.
  16.  梁志远,赵钦新,张智超等.表面渗层和CrNiMo涂层材料的露点腐蚀[J].中国表面工程,2012255):56-61
  17.  梁志远,赵钦新.国产Super304H钢实炉高温腐蚀性能研究[C].工程热物理年会论文集.西安:中国工程热物理学会,2014
  18.  梁志远,赵钦新,姜薇薇等.国产Super304H钢高温服役12000h的蒸汽氧化机理研究[C].第一届全国特种设备安全与节能学术会议.海南:中国特种设备检测研究院,2012